MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® C MC 3440 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
Water Absorption 0.60 %0.60 %
Moisture Absorption 0.200 %0.200 %
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 260 °C
45 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min Volumetric Rate
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 4.0 %4.0 %
Tensile Modulus 2.70 GPa392 ksi
Flexural Strength 105 MPa15200 psi
Flexural Modulus 2.50 GPa363 ksi
Izod Impact, Notched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Comparative Tracking Index 575 V575 V
 >= 600 V>= 600 V
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 115 °C239 °F
Deflection Temperature at 1.8 MPa (264 psi) 103 °C217 °F
Vicat Softening Point 120 °C
@Load 5.10 kg
248 °F
@Load 11.2 lb
rate 50°C/h
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Glow Wire Ignition Temperature  775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
 825 °C
@Thickness 0.750 mm
1520 °F
@Thickness 0.0295 in
Glow Wire Flammability Index  750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
 800 °C
@Thickness 0.750 mm
1470 °F
@Thickness 0.0295 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Xantar® C MC 3652 Polycarbonate
Mitsubishi Xantar® C MC 3650 Polycarbonate
Mitsubishi Xantar® C MC 3433 Polycarbonate
Mitsubishi Xantar® C MC 3700 Polycarbonate
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber

PMITSU9340 / 192004

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.