MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 5425 UHMW Polyethylene Tape
Categories: Polymer; Tape

Material Notes: 3M™ UHMW Polyethylene Tape 5425 is a film coated with a special acrylic adhesive that is resistant to many solvents.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milBacking; ASTM D3752
 81.3 microns3.20 milLiner; ASTM D3752
 127 microns5.00 milTotal without liner; ASTM D3752
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.6 MPa8790 psiASTM D3759
Elongation at Break 100 %100 %ASTM D3759
Peel Strength 0.3287 kN/m1.875 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceTranslucent
Liner55# densified kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 5423 Polyethylene Tape
3M Cold Seal® 5130 (Clear) Polyethylene Tape
3M Cold Seal® 4130 Polyethylene Tape
3M Cold Seal® 3130 Polyethylene Tape
3M 5421 Polyethylene Tape

PMM34556 / 169303

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.