MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Cold Seal® 3130 Polyethylene Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Cold Seal® Polyethylene Tape 3130 is a temporary tape with a self-sealing latex emulsion and feature a self-adhering cohesive coating which bonds to itself and not to the product to be packaged and the result is an airtight pouch that is resistant to moisture, dirt and grease.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.70 MPa247 psiASTM D3759
Elongation at Break 450 %450 %ASTM D3759
Peel Strength 0.153 kN/m0.875 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeNatural rubber latex emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 5423 Polyethylene Tape
3M Cold Seal® 5130 (Clear) Polyethylene Tape
3M Cold Seal® 4130 Polyethylene Tape
3M 5425 UHMW Polyethylene Tape
3M 5421 Polyethylene Tape

PMM34386 / 169133

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.