MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Description

Polytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for molding large automotive parts, such as fascias and air dams. TPP 512 is UV stable, paintable and pigmentable.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
Melt Index of Compound 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength at Break 3500 psiASTM D638
Elongation at Break 650 %ASTM D638
Flexural Modulus 120000 psiASTM D790
Gardner Impact 36.0 J
@Temperature -30.0 °C
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
Buckeye Polymers BP FLEX D 6020 Injection Grade TPO
Buckeye Polymers BP FLEX D 6509 CR Injection Grade TPO
Buckeye Polymers BP FLEX D 6520 UX3 Injection Grade TPO
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade

PASHU292 / 25256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.