MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Description

Polytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion in combination with good impact strength.
Application

Typical applications include automotive claddings and radiator grills. TPP 530 is paintable with conventional TPO paint systems.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inas molded
 0.0090 cm/cm0.0090 in/in± 0.1 after 30 min. at 120°C
Melt Index of Compound 7.0 g/10 min7.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength, Yield 22.1 MPa3200 psiASTM D638
Elongation at Yield 50 %50 %ASTM D638
Flexural Modulus 2.07 GPa300 ksiASTM D790
Gardner Impact 24.3 J
@Temperature -30.0 °C
17.9 ft-lb
@Temperature -22.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C
@Temperature 20.0 °C
28.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Brittleness Temperature -15.0 °C5.00 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow INFUSE™ 9817 Olefin Block Copolymer
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO)
RTP Company Permaprene™ 2800 B-65A Thermoplastic Polyolefin Elastomer (TEO)
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer

PASHU296 / 25260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.