MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics HIP Vitox™ Mac-A999R Bio Technical Ceramic
Categories: Ceramic

Material Notes: A very high purity alumina ceramic, produced specifically for surgical implant devices.

Applications:

  • Joint replacement components
  • Femoral heads to match cup liners of same material or UHMWPE
  • Cup liners

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.980 g/ccfired
Porosity 0.00 %fully dense, nominal
Grain Size 1.2 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 90
Hardness, Vickers 22.1Gpa @ Hv
Modulus of Elasticity 407 GPa
Flexural Strength 380 MPabiaxial
 550 MPa4-point
Fracture Toughness 4.00 MPa-m½KIC (SENB)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.80 µm/m-°C
Specific Heat Capacity 0.800 J/g-°C
Thermal Conductivity 30.4 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.9 %
 
Descriptive Properties
Colorwhite
Comparative Wear DataHIP Vitox®, Cr-Co-Mo Alloy
Th-232 Content<0.4 ppm
U-238 Content<0.4 ppm
Wear Factor0.57 (mm3/Nm)10-7, in physiological saline, against UHMWPE, pin on plate tests
 0.68 (mm3/Nm)10-7, in distilled water, against UHMWPE, pin on plate tests
 0.7 (mm3/Nm)10-7, in distilled water, against UHMWPE, pin-on-disc test
 0.87(mm3/Nm)10-7, in distilled water, against UHMWPE, pin-on-disc test
 1.01 (mm3/Nm)10-7, in calf bovine serum, against UHMWPE, pin on plate tests
 1.12 (mm3/Nm)10-7, in distilled water, against UHMWPE, pin on plate tests
 1.7 (mm3/Nm)10-7, dry, against UHMWPE, pin-on-disc test
 1.81 (mm3/Nm)10-7, in calf bovine serum, against UHMWPE, pin on plate tests
 100 (mm3/Nm)10-9, 5 cycles, Stainless Steel. Wear against UHMWPE, pin-on-disc tests in distilled water to ASTM F732-82.
 3.3 (mm3/Nm)10-9, 5 cycles, HIP Vitox®. Wear against UHMWPE, pin-on-disc tests in distilled water to ASTM F732-82.
 3.4 (mm3/Nm)10-7, dry, against UHMWPE, pin-on-disc test
 3.89(mm3/Nm)10-7, in physiological saline, against UHMWPE, pin on plate tests
Wear Rate0.04 mg/million cycles. Wear against UHMWPE, pin-on-disc tests in distilled water to ASTM F732-82
 1.05mg/million cycles. Wear against UHMWPE, pin-on-disc tests in distilled water to ASTM F732-82

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics HIP Vitox ™ Mac-A999R Bio Aluminum Oxide Ceramic
Morgan Advanced Ceramics HIP Vitox™ Bio-compatible Alumina
Beryllium SR-200
Overview of materials for Silicone Rubber
Overview of materials for Stainless Steel

CMORF8073 / 203550

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.