MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics HIP Vitox ™ Mac-A999R Bio Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: A very high purity alumina ceramic of 99.9% Al2O3 content, produced specifically for surgical implant devices.

Prime Features:

  • Clinical use since 1985
  • Highest levels of QA and traceability
  • Excellent wear resistance - far superior to polyethylene/metal joint systems
  • Very high density and non-porous alumina
  • Ultra fine grain
  • Resistant to extreme chemical environments
  • High mechanical strength
  • Highly cost effective
Typical Applications:
  • Joint replacement components
  • Femoral heads to match cup liners of same material or UHMWPE
  • Cup liners
Production Capabilities:
  • 28mm or 32mm diameter for –4 to +4 neck lengths
  • Femoral heads and cup liners for surgeons’ preferred hip systems.

Information provided by Morgan Advanced Materials

Key Words: Mac-A999R Bio
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.978 g/cc0.1437 lb/in³
Open Porosity 0.00 %0.00 %fully dense, % nominal, apparent
Grain Size 1.2 µm1.2 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell HR45N 9090
Hardness, Vickers 22.1
@Load 1.00 kg
22.1
@Load 2.20 lb
[GPa]
Modulus of Elasticity 407 GPa59000 ksi
Flexural Strength 380 MPa55100 psibiaxial
 550 MPa79800 psi4-point
Fracture Toughness 4.00 MPa-m½3.64 ksi-in½KIC(SENB)
K Factor (Wear Factor) 0.570.57(mm3/Nm)10-7, in physiological saline, against UHMWPE, pin-on-plate test, 3.89 recommended ICRP dose
 0.680.68(mm3/Nm)10-7, in distilled water, against UHMWPE, pin-on plate test, 1.12 recommended ICRP dose
 0.700.70(mm3/Nm)10-7, in distilled water, against UHMWPE, in-on disc test, 0.87 recommended ICRP dose
 1.011.01(mm3/Nm)10-7, in calf bovine serum, against UHMWPE, pin-on-plate test, 1.81 recommended ICRP dose
 1.71.7(mm3/Nm)10-7 dry, against UHMWPE, pin-on-disc tests, 3.4 recommended ICRP dose
 3.33.3(mm3/Nm)10-9, 5M cycles , 100 stainless steel recommended ICRP dose
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.80 µm/m-°C3.78 µin/in-°F
Specific Heat Capacity 0.800 J/g-°C0.191 BTU/lb-°F
Thermal Conductivity 30.4 W/m-K211 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.9 %99.9 %
 
Descriptive Properties
Colorwhite
Physical PropertiesEffective dose, <5 recommended ICRP dose
 Th-232 content
 Tissue dose, 200 recommended ICRP dose
 U-238 content
 wear rate, 1.05 recommended ICRP dose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics HIP Vitox™ Bio-compatible Alumina
Morgan Advanced Ceramics HIP Vitox™ Mac-A999R Bio Technical Ceramic
Morgan Advanced Ceramics Vitox® AMC Alumina Matrix Composite Aluminum Oxide Ceramic
Overview of materials for AISI 9000 Series Steel
Overview of materials for Silicone Rubber

CMORF5023 / 200261

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.