MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco NLGI 2 SRI Grease OEM
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Features

Chevron SRI Grease OEM is a high temperature ball and roller bearing grease.

It is formulated with ISOSYN™ base stocks, a synthetic polyurea ashless organic thickener, and high performance rust and oxidation inhibitors (the latter to provide superior rust protection in severe applications). Its texture is smooth and buttery and its color is dark green.

Chevron SRI Grease OEM is manufactured to meet the stringent requirements of bearing OEMs (Original Equipment Manufacturers). It combines low noise operation, high temperature performance and low shear stability. ASTM D 3336 tests show that the life of a 204 K bearing lubricated with Chevron SRI Grease OEM and operating at 150°C (302°F) and 10,000 rpm is about 3000 hours. This is nearly 10 times the life possible when using conventional lithium greases and about three times that when using sodium greases. It passes ASTM D 1743-73 rust test with 5% synthetic sea water.

Applications

Chevron SRI Grease OEM is recommended:

  • for use in antifriction bearings operating at high speeds (10,000 rpm and greater)
  • where silent operations are required
  • where the operating temperatures are on the order of 150°C (302°F) and higher
  • where there is a likelihood that water or salt water will get into the bearings

It performs satisfactorily in bearings at temperatures as low as -30°C (-22°F).

Applications where Chevron SRI Grease OEM will outperform most other greases include

  • As a “life-pack” lubricant by manufacturers of rolling element bearings, particularly ball bearings.
  • Other applications where silent operations, high temperature performance, or low shear stability are called for.
Bearing Manufacturers that specifically use Chevron SRI Grease OEM are NSK, NTN, FAG, SKF, NMB, GMN, Torrington, Fujikoshi, American Koyo.

Key Words: CPS Number: 254510; MSDS Number: 6979
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 95Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 517 SUS
Saybolt Viscosity at 210°F 63.9 SUS
Kinematic Viscosity at 40°C (104°F) 99 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration 280Worked
 <= 380Worked (100,000 strokes)
Penetration P(0), 1/10 mm 255
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -30.0 °C
Pour Point -15.0 °CASTM D97
Flash Point 260 °CASTM D92
Dropping Point 243 °C
 
Descriptive Properties
ColorDark Green
High Temperature Life, hours at 177°C, ASTM D3336600
Lincoln Ventmeter, psig at 30 s, at 0°F750
Lincoln Ventmeter, psig at 30 s, at 30°F425
Lincoln Ventmeter, psig at 30 s, at 75°F225
TextureSmooth, Buttery
Thickener, % / type8 / Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco NLGI 2 SRI Grease
ChevronTexaco Rykon® 1426 Premium Grease
ChevronTexaco Rykon® 1364 Premium Grease
ChevronTexaco Polystar® CVJ

WCHEV270 / 74885

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.