MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Rykon® 1364 Premium Grease
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Features

Chevron Rykon Premium Grease No. 1364 contains polyurea thickener in highly refined paraffinic oil, as well as extreme pressure and rust protection additives. Chevron Rykon Premium Grease No. 1364:

  • is resistant to oil separation during use and storage.
  • has excellent high temperature characteristics.
  • will not blacken copper or steel when tested for one hour at 150°C (302°F).

Applications

Chevron Rykon Premium Grease No. 1364 was formulated specifically for the automotive constant velocity (CV) driveline joints used in front-wheel drive automobiles.

It is compatible with the common elastomers used for boots in the joints and can be used in "hot" CV joints up to 177°C (350°F).

Chevron Rykon Premium Grease No. 1364 can also be used in other applications requiring a high temperature grease with extreme pressure additives.

Chevron Rykon Premium Grease No. 1364 meets the requirements of GKN specification M-3005 for CV grease.

Key Words: CPS Number: 231056; MSDS Number: 7611
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9090Viscosity Index of base oil; ASTM D2270
Saybolt Viscosity at 100°F 596 SUS596 SUS
Saybolt Viscosity at 210°F 76 SUS76 SUS
Kinematic Viscosity at 40°C (104°F) 115 cSt115 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14.1 cSt14.1 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Penetration 312312Worked
Timken Test 18100 g40.0 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Dropping Point 243 °C469 °F
 
Descriptive Properties
Bearing RustPass
ColorBlue
TextureSmooth
Thickener, % / type10 / Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Rykon® NLGI 1 Premium Grease EP
ChevronTexaco Rykon® 1426 Premium Grease
ChevronTexaco NLGI 2 SRI Grease OEM
ChevronTexaco NLGI 2 SRI Grease
Crucible Steel AISI 52100 Alloy Steel

WCHEV264 / 74879

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.