MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem ES6007 Blown Molding and Injection Blown Molding High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade; High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description: ES6007 is a homopolymer high-density polyethylene developed for the blow-molding segment. Offers excellent stiffness, high productivity and good organoleptic characteristics.

Application: Blow Molded Small Volume: Dairy bottles, yogurt and liquid food packing.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
ESCR 100% Igepal® <= 15 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 55 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaASTM D638
Flexural Modulus, 1% Secant 1550 MPaASTM D790
Izod Impact, Notched 125 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °CBlow Molding
Die Temperature 5.00 - 25.0 °CInjection Blow Molding
 160 °CInjection Blow Molding
 190 °CBlow Molding
Mold Temperature 5.00 - 25.0 °CInjection Blow Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 3282 Injection Grade HDPE
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin
Braskem BU 004 HDPE Blow Molding Polyethylene
Braskem BU004W Blown Molding High Density Polyethylene
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene

PBRASK2083 / 199964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.