MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Description: SGD4960 is a high density polyethylene homopolymer especially designed for blow molding processing. It features high density and stiffness combined with high impact resistance. The minimum biobased content of this grade is 96%, determined according to ASTM D6866.

Application: Bottles for food applications such as dairy products and beverages. Containers for non-food applications such as alcohol, cosmetics and lubricant oils.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D792
ESCR 100% Igepal® 24 hour
@Temperature 50.0 °C
24 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
ESCR 10% Igepal® 19 hour
@Temperature 50.0 °C
19 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow  0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 50 g/10 min
@Load 21.6 kg,
Temperature 190 °C
50 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength at Break 22.0 MPa3190 psiASTM D638
Tensile Strength, Yield 32.0 MPa4640 psiASTM D638
Flexural Modulus, 1% Secant 1600 MPa232000 psiASTM D790
Izod Impact, Notched 0.890 J/cm1.67 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FASTM D648
Vicat Softening Point 128 °C
@Load 1.02 kg
262 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SGF4950HS Blow Molded High Density Polyethylene
Braskem Green PE STN7006 Blown Film Extrusion Low Density Polyethylene
Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene
Braskem Green PE SHE150 High Density Polyethylene
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene

PBRASK2002 / 199884

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.