MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QM 231 30 Shore A, Translucent, Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 231 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material has been designed for the prototyping industry. However, it is also a good choice for the molding of furniture, picture frames and architectural materials.

Key Features:

  • Translucent
  • Fast demold time
  • Excellent physical properties
  • Excellent dimensional stability
  • Casting resin resistance
Main Applications:
  • Molds for rapid prototyping
  • Molds for architectural replication
  • Molds for polyester, epoxy, and rigid or foam polyurethane resin casting
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccQM 231B
 1.10 g/ccQM 231A
Viscosity 800 cPQM 231B
 50000 cPCatalyzed
 70000 cPQM 231A
Linear Mold Shrinkage <= 0.0010 cm/cmCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30Cured
Tensile Strength 700 psiCured
Elongation at Break 511 %Cured
Tear Strength 91.0 pliCured
 
Processing PropertiesOriginal ValueComments
Cure Time 18.0 - 24.0 hourDemold time, Catalyzed
Pot Life 300 minCatalyzed
 
Descriptive Properties
ColorClearQM 231B, Uncatalyzed
 TranslucentCatalyzed
 TranslucentQM 231A, Uncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QM 130T 30 Shore A, Translucent, Condensation Cure Moldmaking Material
CHT Group QM 132T 30 Shore A, Translucent, Condensation Cure Moldmaking Material
CHT Group QLE 1033 30 Shore A, Addition Cure Elastomer for Coating Applications
CHT Group True SkinĀ® 30 30 Shore A, Clear Addition Cure Material
Overview of materials for Silicone Rubber

PACC2047 / 199435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.