MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QM 130T 30 Shore A, Translucent, Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 130T is a two-component, translucent, room temperature, condensation cure, silicone material. When catalyzed with QM Cat Clear Thixo 2 the resulting material is extremely thixotropic. QM 130T is also available for non-thixotropic, flowable applications when catalyzed with QM Cat Clear. The cured rubber has excellent properties and good shelf life stability.

Key Features:

  • High tear strength
  • High thixotropy (if desired)
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for polyester, polyurethane and epoxy resin castings
  • Designed specifically for vacuum bag applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncatalyzed Cat Clear
 1.03 g/cc1.03 g/ccUncatalyzed Clear Thixo 2
 1.12 g/cc1.12 g/ccUncatalyzed QM 130T
 1.13 g/cc1.13 g/ccCatalyzed Cat Clear
 1.13 g/cc1.13 g/ccCatalyzed Clear Thixo 2
Viscosity 100 cP100 cPUncatalyzed Cat Clear
 900 cP900 cPUncatalyzed Clear Thixo 2
 50000 cP50000 cPUncatalyzed QM 130T
Linear Mold Shrinkage <= 0.0030 cm/cm<= 0.0030 in/inCured 3 days RT, Cat Clear
 <= 0.0030 cm/cm<= 0.0030 in/inCured 3 days RT, Catalyzed Clear Thixo 2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030Cured 3 days RT, Cat Clear
 3030Cured 3 days RT, Catalyzed Clear Thixo 2
Tensile Strength 3.45 MPa500 psiCured 3 days RT, Cat Clear
 3.45 MPa500 psiCured 3 days RT, Catalyzed Clear Thixo 2
Elongation at Break 350 %350 %Cured 3 days RT, Catalyzed Clear Thixo 2
 450 %450 %Cured 3 days RT, Cat Clear
Tear Strength 12.3 kN/m70.0 pliCured 3 days RT, Catalyzed Clear Thixo 2
 24.5 kN/m140 pliCured 3 days RT, Cat Clear
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FCured 3 days RT, Cat Clear
 150 °C302 °FCured 3 days RT, Catalyzed Clear Thixo 2
Minimum Service Temperature, Air -50.0 °C-58.0 °FCured 3 days RT, Cat Clear
 -50.0 °C-58.0 °FCured 3 days RT, Catalyzed Clear Thixo 2
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min8.00 - 12.0 hourDemold time, Catalyzed Clear Thixo 2
 720 - 960 min12.0 - 16.0 hourDemold time, Catalyzed Cat Clear
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Cat Clear
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Catalyzed Clear Thixo 2
Tack-Free Time 240 - 300 min4.00 - 5.00 hourCatalyzed Clear Thixo 2
 240 - 360 min4.00 - 6.00 hourCatalyzed Cat Clear
Pot Life 20.0 min20.0 minCatalyzed Cat Clear
 20.0 min20.0 minCatalyzed Clear Thixo 2
 
Descriptive Properties
ColorTranslucentUncatalyzed QM 130T
 TranslucentUncatalyzed Cat Clear
 TranslucentUncatalyzed Clear Thixo 2
 TranslucentCatalyzed Cat Clear
 TranslucentCatalyzed Clear Thixo 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QM 132T 30 Shore A, Translucent, Condensation Cure Moldmaking Material
CHT Group QM 231 30 Shore A, Translucent, Addition Cure Moldmaking Material
CHT Group QLE 1033 30 Shore A, Addition Cure Elastomer for Coating Applications
Overview of materials for Silicone Rubber
RTP Company RTP 2800B-30D  Thermoplastic Vulcanizate Elastomer (TPV) 30 Shore D

PACC2041 / 199429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.