MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Palatinol® 711P Phthalate Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Formula: C26H42O4

Description: Palatinol® 711P is a predominantly linear phthalate plasticizer based upon C7, C9 and C11 alcohols. It is compatible with both homopolymer and copolymer vinyl resins, chlorinated rubber, SBR, neoprene and nitrile rubber as well as cellulosics. Palatinol 711P is used primarily to plasticize vinyl resin where good processing characteristics are needed and the finished product requires improved low temperature flexibility, low volatility or good outdoor weatherability

Applications: Palatinol 711P is an excellent general purpose phthalate plasticizer. With its efficiency, low-volatility, superior low temperature flexibility and good weatherability. The processor can expect: rapid dry blending and fusion, improved thermal stability, higher output (line speed) and better efficiency. The consumer can expect: high gloss finish, outdoor weatherability, thermal stability, low temperature flexibility, good hand, feel and drape. Typical end uses are: swimming pool and pond liners, roofing membranes, coated fabrics, tarpaulins, high-end luggage, exterior automotive trim and building and communication wire.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.965 - 0.973 g/ccASTM D4052
Solubility of Water 0.0020 %
Solubility in Water <= 1.0e-6 %
Viscosity 20 cP
@Temperature 40.0 °C
Absolute
 51 cP
@Temperature 20.0 °C
Absolute
 180 cP
@Temperature 0.000 °C
Absolute
Molecular Weight 418 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.070[mg KOH/g]; ASTM D1045
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 15.0 sec
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
 80
@Time 15.0 sec
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
 88
@Time 15.0 sec
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 12.6 MPaPlasticizer conc. in vinyl film 70 phr; ASTM D638
 16.0 MPaPlasticizer conc. in vinyl film 50 phr; ASTM D638
 18.3 MPaPlasticizer conc. in vinyl film 40 phr; ASTM D638
Elongation at Break 285 %Plasticizer conc. in vinyl film 40 phr; ASTM D638
 320 %Plasticizer conc. in vinyl film 50 phr; ASTM D638
 360 %Plasticizer conc. in vinyl film 70 phr; ASTM D638
100% Modulus 0.875 ksi
@Strain 100 %
Plasticizer conc. in vinyl film 70 phr; ASTM D638
 1.44 ksi
@Strain 100 %
Plasticizer conc. in vinyl film 50 phr; ASTM D638
 1.895 ksi
@Strain 100 %
Plasticizer conc. in vinyl film 40 phr; ASTM D638
Torsional Stiffness 45000 psi
@Temperature -14.0 °C
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
 45000 psi
@Temperature -27.0 °C
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
 45000 psi
@Temperature -41.0 °C
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
 
Thermal PropertiesOriginal ValueComments
CTE, linear 780 µm/m-°C
Boiling Point 238 °C
@Pressure 600000 MPa
Pour Point -50.0 °C
Brittleness Temperature -47.0 °CPlasticizer conc. in vinyl film 70 phr; ASTM D746
 -37.0 °CPlasticizer conc. in vinyl film 50 phr; ASTM D746
 -27.0 °CPlasticizer conc. in vinyl film 40 phr; ASTM D746
Flash Point 227 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.482
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.050 %ASTM E203
 
Descriptive Properties
Color<25APAH, ASTM D5386
CompositionEster content>99.6%, ASTM D3465

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane
BASF Palamoll® 656 Polymeric Plasticizer
BASF Palamoll® 654 Polymeric Plasticizer
Evonik VESTINOL® INB Plasticizer
Evonik VESTINOL® 9 Plasticizer

PBASG0742 / 132375

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.