MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Palatinol® 711P Phthalate Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Formula: C26H42O4

Description: Palatinol® 711P is a predominantly linear phthalate plasticizer based upon C7, C9 and C11 alcohols. It is compatible with both homopolymer and copolymer vinyl resins, chlorinated rubber, SBR, neoprene and nitrile rubber as well as cellulosics. Palatinol 711P is used primarily to plasticize vinyl resin where good processing characteristics are needed and the finished product requires improved low temperature flexibility, low volatility or good outdoor weatherability

Applications: Palatinol 711P is an excellent general purpose phthalate plasticizer. With its efficiency, low-volatility, superior low temperature flexibility and good weatherability. The processor can expect: rapid dry blending and fusion, improved thermal stability, higher output (line speed) and better efficiency. The consumer can expect: high gloss finish, outdoor weatherability, thermal stability, low temperature flexibility, good hand, feel and drape. Typical end uses are: swimming pool and pond liners, roofing membranes, coated fabrics, tarpaulins, high-end luggage, exterior automotive trim and building and communication wire.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.965 - 0.973 g/cc0.0349 - 0.0352 lb/in³ASTM D4052
Solubility of Water 0.0020 %0.0020 %
Solubility in Water <= 1.0e-6 %<= 1.0e-6 %
Viscosity  20 cP
@Temperature 40.0 °C
20 cP
@Temperature 104 °F
Absolute
 51 cP
@Temperature 20.0 °C
51 cP
@Temperature 68.0 °F
Absolute
 180 cP
@Temperature 0.000 °C
180 cP
@Temperature 32.0 °F
Absolute
Molecular Weight 418 g/mol418 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.070<= 0.070[mg KOH/g]; ASTM D1045
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  68
@Time 15.0 sec
68
@Time 0.00417 hour
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
 80
@Time 15.0 sec
80
@Time 0.00417 hour
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
 88
@Time 15.0 sec
88
@Time 0.00417 hour
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 12.6 MPa1830 psiPlasticizer conc. in vinyl film 70 phr; ASTM D638
 16.0 MPa2320 psiPlasticizer conc. in vinyl film 50 phr; ASTM D638
 18.3 MPa2650 psiPlasticizer conc. in vinyl film 40 phr; ASTM D638
Elongation at Break 285 %285 %Plasticizer conc. in vinyl film 40 phr; ASTM D638
 320 %320 %Plasticizer conc. in vinyl film 50 phr; ASTM D638
 360 %360 %Plasticizer conc. in vinyl film 70 phr; ASTM D638
100% Modulus  6.03 MPa
@Strain 100 %
875 psi
@Strain 100 %
Plasticizer conc. in vinyl film 70 phr; ASTM D638
 9.93 MPa
@Strain 100 %
1440 psi
@Strain 100 %
Plasticizer conc. in vinyl film 50 phr; ASTM D638
 13.07 MPa
@Strain 100 %
1895 psi
@Strain 100 %
Plasticizer conc. in vinyl film 40 phr; ASTM D638
Torsional Stiffness  310 MPa
@Temperature -14.0 °C
45000 psi
@Temperature 6.80 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
 310 MPa
@Temperature -27.0 °C
45000 psi
@Temperature -16.6 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
 310 MPa
@Temperature -41.0 °C
45000 psi
@Temperature -41.8 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
 
Thermal PropertiesMetricEnglishComments
CTE, linear 780 µm/m-°C433 µin/in-°F
Boiling Point 238 °C
@Pressure 600000 MPa
460 °F
@Pressure 8.70e+7 psi
Pour Point -50.0 °C-58.0 °F
Brittleness Temperature -47.0 °C-52.6 °FPlasticizer conc. in vinyl film 70 phr; ASTM D746
 -37.0 °C-34.6 °FPlasticizer conc. in vinyl film 50 phr; ASTM D746
 -27.0 °C-16.6 °FPlasticizer conc. in vinyl film 40 phr; ASTM D746
Flash Point 227 °C441 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4821.482
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.050 %0.050 %ASTM E203
 
Descriptive Properties
Color<25APAH, ASTM D5386
CompositionEster content>99.6%, ASTM D3465

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane
BASF Palamoll® 656 Polymeric Plasticizer
BASF Palamoll® 654 Polymeric Plasticizer
Evonik VESTINOL® INB Plasticizer
Evonik VESTINOL® 9 Plasticizer

PBASG0742 / 132375

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.