MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hyosung Topilene R200P PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: Topilene® R200P is a specially designed polypropylene random copolymer (PP-R, natural colored) that features excellent long-term hydrostatic pressure resistance and heat stability. It is suitable for hot & cold water supply pipes and fittings as well as radiator connecting pipes. It is the outcome of HYOSUNG's integrated bimodal polymerization and crystallization technology with advanced PP manufacturing process technique.

Typical Applications: Hot &cold water supply pipes and fittings/ Radiator connecting pipes

Features: Excellent long-term hydrostatic pressure resistance and heat stability (PPR 125, MRS 12.5 MPa, CRS 3.3 MPa)/ Excellent stiffness and impact strength balance / Chemical stability / Environment-friendly / Enhanced processability

Compliance: The pipes produced with Topilene® R200P complies with the hydrostatic pressure requirements according to DIN 8078, ISO/DIS 15874-2, GB/T 18742 and KS M 3362.It complies with the requirements of NSF/ANSI 14, FDA21 CFR 177.1520 and (EU) No 10/2011 for food contact. This product corresponds to the DVGW W270/KTW guidelines and GB/T17219for drinking water system.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 0.25 g/10 min
@Load 0.00000220 kg,
Temperature 230 °C
ASTM D1238
Storage Temperature 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 75ASTM D785
Tensile Strength, Yield 270 kg(f)/cm²ASTM D638
Flexural Modulus 9000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched NBASTM D256
 5.00 kg-cm/cm
@Temperature -10.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µin/in-°F
@Temperature 0.000 - 80.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CASTM D648
Vicat Softening Point 130 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 30.0 °CCooling temperature
 180 - 220 °CMixing zone
Feed Temperature 160 - 180 °C
Die Temperature 180 - 220 °C
Melt Temperature 180 - 210 °CMelting zone
 200 - 230 °C
Head Temperature 180 - 220 °C
Drying Temperature 80.0 - 100 °C
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4042 Polypropylene, Fiber/Filament Grade
LyondellBasell Petrothene FR200000 Polypropylene
304 Stainless Steel
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose
Constellium PLAN 5754 Aluminum Rolled Plate

PHYOS24 / 47910

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.