System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
EMS-Griltech Grilon® BM 10 Nylon 6 Monofilament (Medium-Set)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6 Fiber
Material Notes:
Description:
GRILON BM 10 is a Nylon 6 based monofilament for filtration.
Special Note: GRILON Monofilament has been bought by Shakespeare
Data provided by EMS-Griltech.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.14
g/cc
Filament Diameter
180
-
1000
µm
Mechanical Properties
Original Value
Comments
Elongation at Break
35 - 50 %
Tenacity
0.351
-
0.526
N/tex
Thermal Properties
Original Value
Comments
Melting Point
220
°C
Shrinkage
11 - 14 %
@Temperature 180 °C
Thermo Shrinkage
Descriptive Properties
Heat Setting
Medium-Set
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Akulon® K224-PG6 PA6-I-GF30, Conditioned, 30% Glass Reinforced, Impact Modified
Trinseo PULSE™ A35-105 PC/ABS
INEOS Styrolution Terblend® N NM-21 XP ABS+PA (Dry)
EMS-Griltech Grilon® BM 25R Nylon 6 Monofilament (Medium-Set)
EMS-Griltech Grilon® BM 24R Nylon 6 Monofilament (Medium-Set)
PGRIL399 / 43251
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.