MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo PULSE™ A35-105 PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ A35-105 PC/ABS resin delivering optimized performance for automotive interior component applications

Benefits:

  • High-impact strength even at low temperature
  • High Heat resistance for demanding automotive interior components
  • Consistent natural white color produces high quality part appearance when used with color concentrates (self coloring) or Trinseo Color Masterbatch Technology
  • Low odor & VOC to meet all global Automotive OEM specifications
Application:
  • Mid (floor) consoles
  • Instrument Panel components
  • Door panel trim
  • Pillars
  • Storage/load floors/ glove box
Automotive Specifications:
  • BMW GS 9301
  • DAIMLER DBL 5404.28
  • GM QK 002412 Color: Natural
  • QK 002432
  • JLR STJLR.51.353
  • JLR STJLR.51.5229
  • JLR STJLR.51.5262
  • PSA Peugeot-Citroen ABS/PC-0001
  • VOLKSWAGEN TL 522 31-A
  • VOLVO STD 121.86

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Density 1.12 g/cc0.0405 lb/in³ISO R1183 B
Volatile Organic Compounds (VOC) Content 9.0 g/l9.0 g/lVDA 277
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 260 °C
17 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Spiral Flow 48.0 cm18.9 inMelt Temperature: 260°C, Injection Pressure: 2610 psi
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 52.0 MPa7540 psiISO 527-2/5
Elongation at Break >= 80 %>= 80 %ISO 527-2/5
Tensile Modulus 2.20 GPa319 ksiISO 527-2
Flexural Modulus 2.10 GPa305 ksiISO 178
Charpy Impact, Notched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 80.0 °C
40.0 µin/in-°F
@Temperature 32.0 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °Funannealed; ISO 75 A
Vicat Softening Point 122 °C252 °F50°C/hr, 5 kg; ISO 306 B
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 105 °C221 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ A35-110 PC/ABS
Covestro Bayblend® T65 HG PC/ABS Blend
Envalior Akulon® K224-PG6 PA6-I-GF30, Conditioned, 30% Glass Reinforced, Impact Modified
Covestro Bayblend® T65 XF Polycarbonate + ABS
Trinseo PULSE™ GX50 PC/ABS Engineering Resin

PZZDOW1405 / 30623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.