MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermal Ceramics Cerachrome Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forging furnaces. Cerachrome Blanket with its chromia-stabilized chemistry offers improved long term shrinkage characteristics over zirconia containing blankets such as Cerachem. Cerachrome Blanket effectively fills the gap between zirconia blankets and high alumina products.

Military Specifications and Approvals:

  • Mil-I-23128A- 3, 6 pcf blanket
  • Mil-I-24244- all blankets
  • Mil-I-23128B- 6, 8 pcf blanket
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0640 g/cc0.00231 lb/in³Available in multiple densities
     0.0960 g/cc0.00347 lb/in³Available in multiple densities
     0.128 g/cc0.00462 lb/in³Available in multiple densities
    Thickness 12500 - 50000 microns492 - 1970 mil
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0600 W/m-K
    @Temperature 260 °C
    0.416 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    8 pcf
     0.0700 W/m-K
    @Temperature 260 °C
    0.486 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    6 pcf
     0.0800 W/m-K
    @Temperature 260 °C
    0.555 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    4 pcf
     0.130 W/m-K
    @Temperature 538 °C
    0.902 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    8 pcf
     0.150 W/m-K
    @Temperature 538 °C
    1.04 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    6 pcf
     0.190 W/m-K
    @Temperature 538 °C
    1.32 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    4 pcf
     0.230 W/m-K
    @Temperature 816 °C
    1.60 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    8 pcf
     0.270 W/m-K
    @Temperature 816 °C
    1.87 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    6 pcf
     0.300 W/m-K
    @Temperature 982 °C
    2.08 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    8 pcf
     0.340 W/m-K
    @Temperature 1093 °C
    2.36 BTU-in/hr-ft²-°F
    @Temperature 1999 °F
    8 pcf
     0.350 W/m-K
    @Temperature 982 °C
    2.43 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    6 pcf
     0.360 W/m-K
    @Temperature 816 °C
    2.50 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    4 pcf
     0.410 W/m-K
    @Temperature 1093 °C
    2.85 BTU-in/hr-ft²-°F
    @Temperature 1999 °F
    6 pcf
     0.470 W/m-K
    @Temperature 982 °C
    3.26 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    4 pcf
     0.540 W/m-K
    @Temperature 1093 °C
    3.75 BTU-in/hr-ft²-°F
    @Temperature 1999 °F
    4 pcf
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1370 °C2500 °FContinuous
     1430 °C2600 °FRating
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 43 %43 %
    Cr2O3 3.0 %3.0 %
    SiO2 54 %54 %
     
    Descriptive Properties
    Other Element Contenttraces
    Water Leachable Elements on Surface of Fiber, PPMBoron, 40
     Chlorine, <10
     Fluorine, <5
     Silicate, 125
     Sodium, 40
     Sulfur, 10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
    Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
    Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
    Morgan Advanced Ceramics Denka Alcen NBK80 Thermal Ceramic
    Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

    CTHERM004 / 2324

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.