MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Morgan Advanced Ceramics Denka Alcen NBK80 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: PCW fiber class. Denka Alcen Blankets are made from high alumina fibers using the sol-gel process. They are doubled needled for exceptional strength and flexibility for use in applications up to 2912°F (1600°C) in oxidizing, reducing and chemically aggressing atmospheres.

Applications:

  • Reheat Furnace Linings
  • Galvanizing Furnace Linings
  • Reducing Atmosphere Furnace Linings
  • Aluminum Furnaces
  • High Firing Ceramics Kiln Linings

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
 1.28 g/cc0.0462 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0500 W/m-K
@Temperature 260 °C
0.347 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
 0.110 W/m-K
@Temperature 538 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 0.190 W/m-K
@Temperature 816 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
 0.300 W/m-K
@Temperature 1093 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 1999 °F
ASTM C201
 0.440 W/m-K
@Temperature 1371 °C
3.05 BTU-in/hr-ft²-°F
@Temperature 2500 °F
ASTM C201
Melting Point 2000 °C3630 °F
Shrinkage <= 1.0 %
@Treatment Temp. 1371 °C,
Time 86400 sec
<= 1.0 %
@Treatment Temp. 2500 °F,
Time 24.0 hour
isothermal heating
 
Component Elements PropertiesMetricEnglishComments
Al2O3 80 %80 %
SiO2 20 %20 %
 
Descriptive Properties
Classification Temperature (°C)1600
Colorwhite
Fiber Diameter (um)[3-5]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Thermal Ceramics Cerachrome Blanket
Morgan Advanced Ceramics Cerafelt® RCF Fiber Thermal Ceramic

CMORF6073 / 202857

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.