MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket
Categories: Polymer; Thermoset

Material Notes: SOFT-SHIELD 5500 EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automation equipment, reprographics and grounding applications. A growing number of standard profiles and sizes provide flexibility when selecting a gasket for a specific application. Custom profiles or sizes can also be produced.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Peel Strength >= 0.700 kN/mASTM D1000
Compression Set <= 25 %ASTM D3574
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.0090 ohmInitial, 168 hours @ 185 °F; CHO-TM-TP57
 0.0090 ohmInitial, 168 hours @ 250°F; CHO-TM-TP57
 0.0090 ohmInitial, 168 hours @ 95°F, 95% RH; CHO-TM-TP57
 0.010 ohmInitial, 2190 hours @ 158°F; CHO-TM-TP57
 0.010 ohmFinal, 2190 hours @ 158°F; CHO-TM-TP57
 0.014 ohmFinal, 168 hours @ 95°F, 95% RH; CHO-TM-TP57
 0.014 ohmInitial, 168 hours @ 185 °F; CHO-TM-TP57
 0.017 ohmFinal, 168 hours @ 250°F; CHO-TM-TP57
Shielding Effectiveness >= 70 dB50 MHz to 10 GHz; CHO-TM-TP08
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Taber Abrasion, mg/500 Cycles0.01 ohmsASTM D460

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Stainless Fiber, EMI
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket
Parker Chomerics CHO-MUTE 9020 RF Absorber

PCHOME003 / 28225

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.