MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 19.9.NbSi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.NbSi is a filler metal particularly suited for MIG welding. It can also be used for TIG and plasma arc welding. It is suitable for joining stainless steels of the 18Cr/8Ni/Nb and 18Cr/8Ni/Ti types. Due to the strengthening effect of niobium, this grade is recommended if the weld metal is exposed to temperatures above 400°C (750 F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 225
Tensile Strength, Ultimate 470 MPa
@Temperature 400 °C
 610 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 320 MPa
@Strain 0.2 %,
Temperature 400 °C
 400 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 23 %
@Temperature 400 °C
 35 %
@Temperature 20.0 °C
Reduction of Area 50 %
@Temperature 400 °C
 61 %
@Temperature 20.0 °C
Charpy Impact 60.0 J
@Temperature -196 °C
 110 J
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
 14.0 W/m-K
@Temperature 100 °C
 16.0 W/m-K
@Temperature 200 °C
 18.0 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %AIM
 0.040 %All-Weld Metal
Chromium, Cr 19 %All-Weld Metal
 19.5 %AIM
Cobalt, Co <= 0.20 %AIM
Copper, Cu <= 0.20 %AIM
Manganese, Mn 1.2 %AIM
 1.2 %All-Weld Metal
Molybdenum, Mo <= 0.50 %AIM
Nickel, Ni 10 %AIM
 10 %All-Weld Metal
Niobium, Nb (Columbium, Cb) 0.50 %All-Weld Metal
 >= 0.60 %AIM
Nitrogen, N 0.050 %All-Weld Metal
 <= 0.060 %AIM
Phosphorus, P 0.013 %All-Weld Metal
 <= 0.025 %AIM
Silicon, Si 0.80 %All-Weld Metal
 0.90 %AIM
Sulfur, S 0.010 %All-Weld Metal
 <= 0.015 %AIM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5099 / 199663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.