MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 19.9.NbSi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.NbSi is a filler metal particularly suited for MIG welding. It can also be used for TIG and plasma arc welding. It is suitable for joining stainless steels of the 18Cr/8Ni/Nb and 18Cr/8Ni/Ti types. Due to the strengthening effect of niobium, this grade is recommended if the weld metal is exposed to temperatures above 400°C (750 F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 225225
Tensile Strength, Ultimate  470 MPa
@Temperature 400 °C
68200 psi
@Temperature 752 °F
 610 MPa
@Temperature 20.0 °C
88500 psi
@Temperature 68.0 °F
Tensile Strength, Yield  320 MPa
@Strain 0.2 %,
Temperature 400 °C
46400 psi
@Strain 0.2 %,
Temperature 752 °F
 400 MPa
@Strain 0.2 %,
Temperature 20.0 °C
58000 psi
@Strain 0.2 %,
Temperature 68.0 °F
Elongation at Break  23 %
@Temperature 400 °C
23 %
@Temperature 752 °F
 35 %
@Temperature 20.0 °C
35 %
@Temperature 68.0 °F
Reduction of Area  50 %
@Temperature 400 °C
50 %
@Temperature 752 °F
 61 %
@Temperature 20.0 °C
61 %
@Temperature 68.0 °F
Charpy Impact  60.0 J
@Temperature -196 °C
44.3 ft-lb
@Temperature -321 °F
 110 J
@Temperature 20.0 °C
81.1 ft-lb
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
10.0 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity  13.0 W/m-K
@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 14.0 W/m-K
@Temperature 100 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 212 °F
 16.0 W/m-K
@Temperature 200 °C
111 BTU-in/hr-ft²-°F
@Temperature 392 °F
 18.0 W/m-K
@Temperature 500 °C
125 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.040 %0.040 %AIM
 0.040 %0.040 %All-Weld Metal
Chromium, Cr 19 %19 %All-Weld Metal
 19.5 %19.5 %AIM
Cobalt, Co <= 0.20 %<= 0.20 %AIM
Copper, Cu <= 0.20 %<= 0.20 %AIM
Manganese, Mn 1.2 %1.2 %AIM
 1.2 %1.2 %All-Weld Metal
Molybdenum, Mo <= 0.50 %<= 0.50 %AIM
Nickel, Ni 10 %10 %AIM
 10 %10 %All-Weld Metal
Niobium, Nb (Columbium, Cb) 0.50 %0.50 %All-Weld Metal
 >= 0.60 %>= 0.60 %AIM
Nitrogen, N 0.050 %0.050 %All-Weld Metal
 <= 0.060 %<= 0.060 %AIM
Phosphorus, P 0.013 %0.013 %All-Weld Metal
 <= 0.025 %<= 0.025 %AIM
Silicon, Si 0.80 %0.80 %All-Weld Metal
 0.90 %0.90 %AIM
Sulfur, S 0.010 %0.010 %All-Weld Metal
 <= 0.015 %<= 0.015 %AIM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5099 / 199663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.