MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 2956 is recommended for the bonding and sealing of electronic components where a combination of electrical and mechanical properties are required. This two-part, smooth, paste system of silver filled epoxy is free of solvents and copper or carbon additives. It develops strong durable electrically and thermally conducting bonds and coatings between a number of materials such as metals, ceramics, glass and plastic laminates. TRA- DUCT 2956 cures at room temperature, which makes it extremely useful for bonding heat sensitive components where hot-soldering is impractical. Other common uses include the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields. It is an excellent product for dot dispensing through needles as small as 6 mils.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.40 g/cc2.40 g/ccMixed
Viscosity 145000 cP
@Temperature 25.0 °C
145000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Adhesive Bond Strength 6.89 MPa1000 psiLap shear, alum to alum, 2 min @ 150°C
 6.89 MPa1000 psiLap shear, alum to alum, 5 min @ 100°C
 6.89 MPa1000 psiLap shear, alum to alum, 72 hrs @ 25°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00010 ohm-cm0.00010 ohm-cmcured 72 hrs @ 25°C
 0.00020 ohm-cm0.00020 ohm-cmcured 5 min @ 100°C
 0.00050 ohm-cm0.00050 ohm-cmcured 2 min @ 150°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.0 µm/m-°C
@Temperature 20.0 °C
27.2 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 47.0 °C117 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 150 °C
0.0333 hour
@Temperature 302 °F
 5760 min
@Temperature 25.0 °C
96.0 hour
@Temperature 77.0 °F
Pot Life 720 min720 min
 
Descriptive Properties
Color Silver
Mix Ratio, parts by weight100/6Resin/Hardener
Thixotropic Index 3.95 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-DUCT 916 Epoxy Adhesive
Overview of materials for Epoxy, Electrically Conductive
Overview of materials for Epoxy Adhesive
Atom Adhesives AA-DUCT 2919 Epoxy Adhesive
Overview of materials for Cyanoacrylate Adhesive

PTRAC092 / 71020

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.