MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik H6F Extra-fine Grain Cemented Carbide for Printed Circuit Board Printing  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK H6F extra-fine grain cemented carbide grades has been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

SANDVIK extra-fine grain cemented carbide grades are true sub micron grain size tungsten carbide alloys. The tungsten carbide grain size is 0.8 µm, which is precisely controlled. These grades offer an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

SANDVIK grade H6F incorporates 6% cobalt (Co) and 94% tungsten carbide (WC).

SANDVIK grade H6F is recommended for solid carbide rotary tool applications in the ISO K05/K10 range with special advantages where exceptionally sharp edge profiles are demanded.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.9 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 93.2
Hardness, Vickers 177530
Flexural Strength 4000 MPaTransverse Rupture; ISO 3327
Compressive Strength 7050 MPa
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 6.0 %
WC 94 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
Rogers Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
Rogers Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate

NSANDV026 / 18920

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.