MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with a broad processing window particularly suitable for the preparation of spiral tubing, pneumatic tubing, belting and technical moldings.

Performance Features:

  • High tensile strength
  • Excellent wear performance
  • Excellent hydrolysis resistance
  • Good low temperature flexibility

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccInjection molded parts; ASTM D792
Linear Mold Shrinkage 0.0090 in/inInjection molded; ASTM D955
Melt Index of Compound 33 g/10 min
@Load 10.0 kg,
Temperature 210 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91Injection molded parts; ASTM D2240
Hardness, Shore D 42Injection molded parts; ASTM D2240
Tensile Strength at Break 49.0 MPaInjection molded parts; DIN 53504
Elongation at Break 590 %Injection molded parts; DIN 53504
100% Modulus 0.00750 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.0160 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 660 pliInjection molded parts; ASTM D624
Abrasion 25mm3, Injection molded; DIN 53516
Compression Set 25 %
@Temperature 22.8 °C,
Time 252000 sec
Injection molded; ASTM D395
 39 %
@Temperature 70.0 °C,
Time 86400 sec
Injection molded; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 188 °Cpeak; 0.025" extruded film
 180 - 200 °C0.025" extruded film,
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Middle Barrel Temperature 200 - 210 °CExtrusion
Nozzle Temperature 200 - 210 °CExtrusion
 210 - 225 °CInjection
Adapter Temperature 200 - 210 °CExtrusion
Die Temperature 200 - 210 °CExtrusion
Melt Temperature 205 - 220 °CInjection
Mold Temperature 20.0 - 70.0 °CInjection
 
Descriptive Properties
Heating Zone190-220°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade

PHUQ101 / 159474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.