MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and easy demolding.

Performance Features:

  • Good melt flow
  • Easy demolding
  • Short cycle times
  • Easy coloring recyclable
Applications: For the production of technical parts, wheels and rollers, cover plates, coupling halves, conveyor rollers.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inASTM D995
Melt Index of Compound 90 g/10 min
@Load 10.0 kg,
Temperature 210 °C
90 g/10 min
@Load 22.0 lb,
Temperature 410 °F
cm3/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Hardness, Shore D 4545ASTM D2240
Tensile Strength at Break 45.0 MPa6530 psiDIN 53504
Elongation at Break 690 %690 %ASTM D412
100% Modulus 11.1 MPa
@Strain 100 %
1610 psi
@Strain 100 %
DIN 53504
300% Modulus 19.8 MPa
@Strain 300 %
2870 psi
@Strain 300 %
DIN 53504
Rebound 30 %30 %Bayshore; ASTM D2632
Tear Strength 151 kN/m860 pliASTM D624
Abrasion 3030[mm3]; ISO 4649
Compression Set  24 %
@Temperature 23.0 °C,
Time 252000 sec
24 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 43 %
@Temperature 70.0 °C,
Time 86400 sec
43 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 180 - 190 °C356 - 374 °FHuntsman/TMA
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Front Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °FInjection
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade

PHU9911 / 150371

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.