MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aperam Resistohm® PRM Resistant Alloys Iron-Chromium-Aluminium Alloys
Categories: Metal; Ferrous Metal

Material Notes: This alloy finds his ideal application area for the manufacture of heating elements for industrial furnaces until temperature of 1400 °C. It allows loading rates of about 30 % more than the other FeCrAl alloys. His exceptional life time is due to a very high purity of the metal used which has been melted by electroslag.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.10 g/cc0.257 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 230230
Tensile Strength 750 MPa109000 psi
Tensile Strength, Yield 550 MPa79800 psi
Elongation at Break >= 18 %>= 18 %on 100 mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000145 ohm-cm0.000145 ohm-cmTemperature coefficient = 0.000033/°C from 20 - 100°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.1 µm/m-°C
@Temperature 20.0 - 1000 °C
8.39 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 16.0 W/m-K
@Temperature 120 °C
111 BTU-in/hr-ft²-°F
@Temperature 248 °F
Melting Point 1500 °C2730 °F
Maximum Service Temperature, Air 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Chromium, Cr 23 %23 %
Iron, Fe 71 %71 %
 
Descriptive Properties
Creeping point1.5at 1000°C
 8at 800°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
Aperam Resistohm® 145 Resistant Alloys Iron-Chromium-Aluminium Alloys
Magnesium AS21X1, Die Cast
AISI 1018 Steel, cold drawn
Aperam Resistohm® 135 Resistant Alloys Iron-Chromium-Aluminium Alloys

NPERA092 / 194881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.