MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 2000 / 2120 System 2000 Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical properties of carbon fiber, Kevlar®, and glass laminates! Test results have proven superiority over other room temperature epoxies. Its low viscosity and great handling characteristics make it a favorite in the shop too!

Three high performance hardener systems are available for the System 2000 resin. 20 minute, 60 minute, and 120 minute pot life versions are all options. This added variety allows the fabricator to select the system best suited to the size, complexity or time-frame of the project. Simple parts which need to be demolded quickly should use the 20 minute hardener. Larger and more complex parts can use either of the other hardeners.

Vacuum bagging applications would typically warrant the longest 2 hour working time. As with any epoxy system, adhere to the proper mix ratios and maintain an adequate curing temperature of at least 70°F. The cure time will be cut in half for every 10°F that the temperature is raised above 70°F.

The long pot life 2120 hardener extends working time on large-scale and complex projects. Suitable for vacuum bagging and laminating in hot climates. The 24-36 hour demold time can be reduced by increasing the cure temperature. The post cured service temperature exceeds 200°F.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 - 1.13 g/cc
Viscosity 925 cPASTM D2293
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87Cured; ASTM D2240
Tensile Strength at Break 45870 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638
Elongation at Break 1.98 %Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638
Tensile Modulus 2.52e+6 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
Flexural Strength 66667 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Flexural Modulus 3.05e+6 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.5 µin/in-°F
@Temperature 37.8 - 65.6 °C
ASTM D696
Glass Transition Temp, Tg 194 °F
 
Processing PropertiesOriginal ValueComments
Pot Life 120 min
@Temperature 25.0 °C
4 fl. Oz.; ASTM D2471
 
Descriptive Properties
ColorAmber
Mix Ratio100:27Resin:Hardener by Weight
 3:1Resin:Hardener by Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fibre Glast 2000 / 2020 System 2000 Epoxy
Fibre Glast Epolite 2427 Epoxy
Fibre Glast RAE 2426 / 2177 Epoxy
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled

PFIBRE04 / 38283

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.