MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Categories: Polymer; Thermoset; Epoxy

Material Notes: This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag houses, cyclones, hoppers and other process equipment used in the power, pulp and paper, and chemical processing industries.

Key Words: High Temperature Coatings
Vendors: Aremco’s Corr-Paint™ epoxy and urethane-based coatings are used for producing corrosion and wear resistant barriers. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag houses, cyclones, hoppers and other process equipment. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/cc
Solids Content 100 %100 %weight
 100 %100 %volume
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Thickness >= 1270 microns>= 50.0 milestimated wet film thickness
 >= 1270 microns>= 50.0 milrecommended dry film thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686for Epoxy Coating
Elongation at Break 3.0 %3.0 %for Epoxy Coating
Flexural Strength 92.4 MPa13400 psifor Epoxy Coating
Compressive Strength 71.0 MPa10300 psifor Epoxy Coating
Adhesive Bond Strength  2.07 MPa
@Temperature 175 °C
300 psi
@Temperature 347 °F
Lap Shear Strength vs. Aluminum
 6.21 MPa
@Temperature 150 °C
900 psi
@Temperature 302 °F
Lap Shear Strength vs. Aluminum
 12.4 MPa
@Temperature 100 °C
1800 psi
@Temperature 212 °F
Lap Shear Strength vs. Aluminum
 18.6 MPa
@Temperature 25.0 °C
2700 psi
@Temperature 77.0 °F
Lap Shear Strength vs. Aluminum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourTouch
 12.0 - 14.0 hour12.0 - 14.0 hourHandling
 4.00 - 48.0 hour4.00 - 48.0 hourRecoat
Cure Time  240 min
@Temperature 79.4 °C
4.00 hour
@Temperature 175 °F
>2 Hour Air Set Required Prior to Curing
 2880 min
@Temperature 22.2 °C
48.0 hour
@Temperature 72.0 °F
>2 Hour Air Set Required Prior to Curing
Pot Life 42.0 min
@Temperature 23.0 °C
42.0 min
@Temperature 73.4 °F
Shelf Life 12.0 Month
@Temperature 23.0 °C
12.0 Month
@Temperature 73.4 °F
 
Descriptive Properties
ColorBrown-Red
Dry Film Coverage ft2/gal1604at 1 mil
Mix Ratio1:1Epoxy:Phenolic
Mix Ratio by Weight1:1resin:activator
Mixed ViscosityPaste
PrimerNot Required or Recommended
ThinnerNot Required or Recommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy, Cycloaliphatic, Molded
Mateck Zero Expansion Glass - ZERODUR
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing

PAREM68 / 609

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.