MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtral™ Performance Polyolefin CMV210S Polypropylene Compound
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance, good stiffness/toughness, and UV resistance are required.

Availability:  Africa & Middle East, Europe.  Features: good stiffness, high scratch resistance, medium flow.. Applications: automotive interior trim and parts, automotive applications.   Appearance:  colors available.  Forms: pellets.  Processing Method: injection molding.

Exxtral™ performance polyolefins are high-performance, specialty TPO polypropylene-based compounds. Available in OEM-specific colors with or without UV stabilization, they are lightweight and tough, and offer optimal balance between stiffness and impact resistance in semi-structural and non-structural applications. They are designed to replace higher-cost and heavier materials traditionally used in automobile parts. Benefits include enhanced visual appeal and function of interior vehicle components; aesthetic and safety advantages for exterior parts; performance characteristics that meet the high demands of the tough under the hood environment, and improved design flexibility with multiple grades and custom compounding.

Information provided by ExxonMobil.

Key Words: ExxonMobil™ Performance Polyolefin CMV210S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3610 psiISO 527-2
Elongation at Yield 4.0 %ISO 527-2
Tensile Modulus 305000 psiISO 527-2
Flexural Modulus 326000 psiISO 178
Izod Impact, Notched 3.40 ft-lb/in
@Temperature 22.8 °C
complete break; ISO 180/A
Charpy Impact, Notched 3.80 ft-lb/in²
@Temperature 22.8 °C
complete break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 212 °FISO-75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 131 °FISO-75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil ExxonMobil™ Performance Polyolefin BNV004A Polypropylene Compound
ExxonMobil ExxonMobil™ Performance Polyolefin BMV214 Polypropylene Compound
ExxonMobil Exxtral™ Performance Polyolefin CMV101A Polypropylene Compound
ExxonMobil ExxonMobil™ Performance Polyolefin CNW001A Polypropylene Compound
ExxonMobil ExxonMobil™ Performance Polyolefin CMU205 Polypropylene Compound

PEX98988 / 238369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.