A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior trim applications and UV stabilized. Availability: Africa & Middle East, Europe. Features: good flow, good processability. Applications: automotive interior trim. Appearance: colors available. Forms: pellets. Processing Exxtral™ performance polyolefins are high-performance, specialty TPO polypropylene-based compounds. Available in OEM-specific colors with or without UV stabilization, they are lightweight and tough, and offer optimal balance between stiffness and impact resistance in semi-structural and non-structural applications. They are designed to replace higher-cost and heavier materials traditionally used in automobile parts. Benefits include enhanced visual appeal and function of interior vehicle components; aesthetic and safety advantages for exterior parts; performance characteristics that meet the high demands of the tough under the hood environment, and improved design flexibility with multiple grades and custom compounding. Method: injection molding. Information provided by ExxonMobil. |
ExxonMobil™ Performance Polyolefin CMV101A |