MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
n-Heptane, C7H16
Categories: Fluid; Solvent

Key Words: C7H16
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.684 g/cc
@Temperature 20.0 °C
Viscosity 0.409 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 100.205 g/mol
Vapor Pressure 35.551 torr
@Temperature 20.0 °C
Surface Tension 19.7 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 27.0 atm
Critical Temperature 267 °C
Critical Density 0.232 g/cc
Critical Molar Volume 432 cm³/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.925
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 316.3 J/g
Specific Heat Capacity 2.245 J/g-°C
 1.656 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.124 W/m-K
@Temperature 20.0 °C
Melting Point -90.6 °C
Boiling Point 98.5 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.388
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8737
Antoine's Vapor Pressure B Parameter2911.32
Antoine's Vapor Pressure C Parameter-56.51
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)142-82-5
Chemical FormulaC7H16
Critical Compressibility (Zc)0.263
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A436.73
Dynamic Viscosity Parameter B232.53
Henry's Law Constant (atm m3/mol)0.000259
Molar Heat Capacity (298K)165.918 J/mol-K
Molar Heat Capacity of Vapor a Parameter-5.1421
Molar Heat Capacity of Vapor b Parameter0.6757
Molar Heat Capacity of Vapor c Parameter-0.0003648
Molar Heat Capacity of Vapor d Parameter7.653E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1206
UV cut-off (nm)197

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexane (C6H14)
2-Methylbutane, C5H12
Acetylene, Ethyne, C2H2
Butane (C4H10)
Ethane, C2H6

VORGS185 / 99557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.