MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polycarbonate (PC); Polyurethane, TP; Polycarbonate-Urethane

Material Notes: ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elastomers are manufactured under strict GMP conditions specifically synthesized to overcome the in vivo formation of stress-induced microfissures. Surface microfissuring is a major weakness of present polyurethane elastomers which may lead to catastrophic failures in long-term implanted devices. This makes ChronoFlex® AL an excellent material choice for medical device applications requiring long term durability.

Information provided by AdvanSource Biomaterials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
Tensile Strength, Ultimate 8400 psi
Elongation at Break 325 %
100% Modulus 2.90 ksi
@Strain 100 %
 
Processing PropertiesOriginal ValueComments
Zone 1 390 °F
Zone 2 410 °F
Zone 3 415 °F
Die Temperature 415 °F
Melt Temperature 430 °F
Drying Temperature 160 - 185 °For lower with overnight predrying
Dry Time 3 - 4 hour
Moisture Content <= 0.10 %
Dew Point -40.0 °C
 
Descriptive Properties
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
Titanium Ti-6Al-4V (Grade 5), Annealed

PCARDI01 / 27925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.