MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries Spheriglass® 6000E Solid Glass Spheres  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:
  • Low Uniform Shrinkage
  • Low Warpage
  • High Flexural Modulus
  • High Abrasion Resistance
  • High Compressive Strength
  • Increased Surface Hardness
  • Better Stress Distribution

These and other characteristics enable the spheres to be used in a wide range of applications in the automotive, chemical, electronic, industrial, engineering, and photographic industries.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.54 g/cc
Bulk Density 57.0 lb/ft³Untapped; ASTM D 3101-78
 90.0 lb/ft³Tapped; ASTM D 3101-78
Oil Absorption 20 %ASTM D1483
Particle Size 3.0 µm10% finer than
 7.0 µmmean value
 8.0 µm50% finer than
 15 µm90% finer than
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.5
Modulus of Elasticity 10500 ksi
Coefficient of Friction 1.0
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 - 1.00e+16 ohm-cm
Dielectric Constant 5.8
@Frequency 1e+6 Hz
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.80 µm/m-°C
@Temperature 20.0 °C
Softening Point 846 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55
 
Component Elements PropertiesOriginal ValueComments
Al2O3 14.5 %
B2O3 8.6 %
CaO 22.5 %
Fe2O3 0.20 %
Free Iron <= 0.10 %
K2O 0.20 %
MgO 1.2 %
Na2O 0.30 %
SiO2 52.5 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potters Industries Ballotini® AAA Metal Finishing Glass Bead
Potters Industries Premium 1.5 mm Solid Glass Spheres
Potters Industries Spheriglass® 3000E Solid Glass Spheres
Potters Industries SHERIGLASS® Type I Solid Glass Spacer Bead
Potters Industries Premium 5 mm Solid Glass Spheres

CPOT05 / 1743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.