MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries Spheriglass® 3000E Solid Glass Spheres
Categories: Ceramic; Glass; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:
  • Low Uniform Shrinkage
  • Low Warpage
  • High Flexural Modulus
  • High Abrasion Resistance
  • High Compressive Strength
  • Increased Surface Hardness
  • Better Stress Distribution

These and other characteristics enable the spheres to be used in a wide range of applications in the automotive, chemical, electronic, industrial, engineering, and photographic industries.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.54 g/cc2.54 g/cc
Bulk Density 1.31 g/cc0.0475 lb/in³Untapped; ASTM D 3101-78
 1.60 g/cc0.0579 lb/in³Tapped; ASTM D 3101-78
Oil Absorption 18 %18 %ASTM D1483
Particle Size 30 - 50 µm30 - 50 µmmean value
Particle Mesh Size 325 Mesh325 Mesh
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.56.5
Modulus of Elasticity 72.4 GPa10500 ksi
Coefficient of Friction 1.01.0
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 - 1.00e+16 ohm-cm1.00e+13 - 1.00e+16 ohm-cm
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.80 µm/m-°C
@Temperature 20.0 °C
1.56 µin/in-°F
@Temperature 68.0 °F
Softening Point 846 °C1550 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 14.5 %14.5 %
B2O3 8.6 %8.6 %
CaO 22.5 %22.5 %
Fe2O3 0.20 %0.20 %
Free Iron <= 0.10 %<= 0.10 %
K2O 0.20 %0.20 %
MgO 1.2 %1.2 %
Na2O 0.30 %0.30 %
SiO2 52.5 %52.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Spheriglass® 3000 Solid Glass Spheres
Potters Industries Ballotini® AAA Metal Finishing Glass Bead
Potters Industries Premium 1.5 mm Solid Glass Spheres
Overview of materials for Polypropylene, Film Grade
Overview of materials for Polyester Film

CPOT03_a / 147480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.