MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chicago Extruded Metals UNS C48500 Copper-Zinc-Tin Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Copper-Zinc-Tin Alloy (Naval Brass)

Finished product available as bar, rod, forged, or shapes.
Chicago Extruded Metal temper codes: H01, H02

Information provided by Chicago Extruded Metals

Key Words: CDA 485, ASTM B21, ASTM B124
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.44 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 55 - 8255 - 82
Tensile Strength 393 - 517 MPa57000 - 75000 psi
Tensile Strength, Yield 172 - 365 MPa25000 - 53000 psi
Elongation at Break 15 - 40 %15 - 40 %
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000663 ohm-cm0.00000663 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 116 W/m-K804 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 62 %59 - 62 %
Iron, Fe 0.10 %0.10 %
Lead, Pb 1.3 - 2.2 %1.3 - 2.2 %
Other, total 0.40 %0.40 %
Tin, Sn 0.50 - 1.0 %0.50 - 1.0 %
Zinc, Zn 34.3 - 38.7 %34.3 - 38.7 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium leaded naval brass, UNS C48200, H01 Temper 38 mm bar
ASTM A485 Steel, Grade 1
Medium leaded naval brass, UNS C48200, O60 Temper 25 mm rod
Mueller Alloy 3600 Free Cutting Brass (UNS C36000)
Free-Cutting Brass, UNS C36000

NCHICA918 / 147637

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.