MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mueller Alloy 3600 Free Cutting Brass (UNS C36000)
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Machinability: Recently amended and revised to reflect a lower maximum lead percentage; C36000 remains the industry standard for general machining and high volume production. The excellent machinability characteristic of C36000 permits full utilization of a screw machine’s capabilities.

Workability: Alloy C36000 has a poor capacity to be hot worked. It can be moderately cold worked. However, it is recommended that this be followed by stress relieving at 500 degrees for 1.5 hours to reduce the possibility of stress corrosion cracking.

Applications: Free Cutting Brass include general machining and high volume production where the alloy’s excellent machinability can permit full utilization of the screw machine’s capabilities. With the lower maximum lead content, manufacturers are afforded greater latitude in their designs for lead free compliant component and products. Typical applications include plumbing components and products, fittings, adapters, valve stems, and miscellaneous screw machine parts.

Information Provided by Mueller Industries Inc.

Key Words: ASTM B16, SAE J463, UNS C36000, AMS Alloy 4610
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7272
Tensile Strength at Break 386 MPa56000 psi
Tensile Strength, Yield 310 MPa45000 psi
Elongation at Break 25 %25 %
Machinability 100 %100 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relieving
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 60 - 63 %60 - 63 %
Iron, Fe <= 0.35 %<= 0.35 %
Lead, Pb 2.5 - 3.0 %2.5 - 3.0 %
Zinc, Zn 33.7 - 37.5 %33.7 - 37.5 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Free-Cutting Brass, UNS C36000, Annealed Rod
203 EZ Austenitic Stainless Steel, UNS S20161 (Composition Spec)
Free-Cutting Brass, UNS C36000, H01 (Cold Drawn 15%) Temper shapes
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 25%) Temper 6 mm rod

NMUEL902 / 97690

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.