MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness promotes die life and minimizes failures due to cracking. Remelted and specially refined, PDCQ is an extremely clean steel which can be polished to a critical finish for injection molds. PDCQ is tested by an independent metallurgical laboratory for certification of the microstructural quality rating and toughness measurements.

Information provided by Crucible Industries

Key Words: AISI H13
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 192 - 235
Hardness, Rockwell C 33
@Tempering Temp. 649 °C
air cooled from 1875°F then tempered
 40
@Tempering Temp. 621 °C
air cooled from 1875°F then tempered
 47
@Tempering Temp. 593 °C
air cooled from 1875°F then tempered
 52
@Tempering Temp. 538 °C
air cooled from 1875°F then tempered
Modulus of Elasticity 30000 ksi
Charpy Impact 9.00 ft-lb
@Tempering Temp. 538 °C
air cooled from 1875°F then tempered; V-notch
 9.00 ft-lb
@Tempering Temp. 566 °C
air cooled from 1875°F then tempered; V-notch
 13.0 ft-lb
@Tempering Temp. 579.4 °C
air cooled from 1875°F then tempered; V-notch
 14.0 ft-lb
@Tempering Temp. 593 °C
air cooled from 1875°F then tempered; V-notch
 14.0 ft-lb
@Tempering Temp. 649 °C
air cooled from 1875°F then tempered; V-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.10 µin/in-°F
@Temperature 21.1 - 93.3 °C
 6.40 µin/in-°F
@Temperature 93.3 - 204 °C
 6.80 µin/in-°F
@Temperature 204 - 427 °C
 7.00 µin/in-°F
@Temperature 427 - 538 °C
 7.30 µin/in-°F
@Temperature 538 - 649 °C
Thermal Conductivity 180 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 192 BTU-in/hr-ft²-°F
@Temperature 316 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1560 °FCritical Thermal Treatment Temperature
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 5.2 %
Iron, Fe 90.8 %as balance
Manganese, Mn 0.35 %
Molybdenum, Mo 1.3 %
Silicon, Si 1.0 %
Sulfur, S <= 0.0030 %
Vanadium, V 0.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe LSS™ H10 Hot Work Tool Steel (ASTM H10)
Crucible Steel CHRO-MOW® Tool Steel, AISI H12
Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)
Latrobe LSS™ H12 Hot Work Tool Steel (ASTM H12)
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11

NCRUC936 / 160387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.