MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crucible Steel CHRO-MOW® Tool Steel, AISI H12
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants are used. It may be used up to tool temperatures of about 1000F, with brief exposures up to about 1100F.

Information provided by Crucible Industries

Key Words: AISI H12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192 - 235192 - 235
Hardness, Rockwell C  30 - 32
@Tempering Temp. 621 °C
30 - 32
@Tempering Temp. 1150 °F
air cooled from 1850°F then tempered
 40 - 42
@Tempering Temp. 593 °C
40 - 42
@Tempering Temp. 1100 °F
air cooled from 1850°F then tempered
 44 - 46
@Tempering Temp. 566 °C
44 - 46
@Tempering Temp. 1050 °F
air cooled from 1850°F then tempered
 51 - 53
@Tempering Temp. 538 °C
51 - 53
@Tempering Temp. 1000 °F
air cooled from 1850°F then tempered
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact  10.8 J
@Tempering Temp. 538 °C
8.00 ft-lb
@Tempering Temp. 1000 °F
air cooled from 1850°F then tempered; V-notch
 14.9 J
@Tempering Temp. 566 °C
11.0 ft-lb
@Tempering Temp. 1050 °F
air cooled from 1850°F then tempered; V-notch
 17.6 J
@Tempering Temp. 593 °C
13.0 ft-lb
@Tempering Temp. 1100 °F
air cooled from 1850°F then tempered; V-notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 21.1 - 93.3 °C
6.10 µin/in-°F
@Temperature 70.0 - 200 °F
 11.7 µm/m-°C
@Temperature 21.1 - 204 °C
6.50 µin/in-°F
@Temperature 70.0 - 400 °F
 12.6 µm/m-°C
@Temperature 21.1 - 427 °C
7.00 µin/in-°F
@Temperature 70.0 - 800 °F
 13.3 µm/m-°C
@Temperature 21.1 - 649 °C
7.40 µin/in-°F
@Temperature 70.0 - 1200 °F
Thermal Conductivity  24.2 W/m-K
@Temperature 93.3 °C
168 BTU-in/hr-ft²-°F
@Temperature 200 °F
 25.9 W/m-K
@Temperature 316 °C
180 BTU-in/hr-ft²-°F
@Temperature 600 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 835.0 °C1535 °FCritical Thermal Treatment Temperature
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.35 %0.35 %
Chromium, Cr 5.0 %5.0 %
Iron, Fe 90.45 %90.45 %as balance
Manganese, Mn 0.35 %0.35 %
Molybdenum, Mo 1.3 %1.3 %
Silicon, Si 1.0 %1.0 %
Tungsten, W 1.2 %1.2 %
Vanadium, V 0.35 %0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe LSS™ H10 Hot Work Tool Steel (ASTM H10)
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Latrobe LSS™ H12 Hot Work Tool Steel (ASTM H12)
Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11

NCRUC935 / 160386

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.