MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: Made by adding aluminum to the molten steel and may be used in drawing applications.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 331 MPa.0275 - .035 inches sheet thickness; ASTM A 370
Tensile Strength, Yield 221 MPa.0275 - .035 inches sheet thickness; ASTM A 370
Elongation at Break 40 %.0275 - .035 inches sheet thickness; ASTM A 370
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000142 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.481 J/g-°C
@Temperature 50.0 - 100 °C
 
Descriptive Properties
Deep-Drawing Capability rm1.4.0275 - .035 inches sheet thickness
Strain Hardening Exponent n0.21.0275 - .035 inches sheet thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Deep Drawing Steel (DDS Type B), Standard Grade
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (FS Type B), Standard Grade

NAKS059 / 14662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.