MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UNS C99600, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand.

Applications: Damping alloy to reduce noise and vibration.

As cast values below are for sand casting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.23 g/cc0.297 lb/in³Estimated
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1301303000 kg
Hardness, Rockwell B 7272
Tensile Strength, Ultimate 558 MPa80900 psias cast
 558 MPa80900 psiheat treated
Tensile Strength, Yield 248 MPa36000 psias cast
 303 MPa43900 psiheat treated
Elongation at Break 27 %27 %heat treated
 34 %34 %as cast
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.0 %2.0 %
Copper, Cu 58 %58 %
Manganese, Mn 40 %40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UNS C99750, Copper Casting Alloy
NDZ-S, UNS C99500, Copper Casting Alloy
Nondezincification Alloy, UNS C99400, Copper Casting Alloy
UNS C94000, Copper Casting Alloy
UNS C94100, Copper Casting Alloy

MC99600b1 / 11986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.