MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nondezincification Alloy, UNS C99400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, and Sand.

Applications: Valve stems, marine and other uses requiring resistance to dezincifications and dealuminification, propeller wheels, electrical parts, mining equipment gears.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125125M01 temper; 3000 kg
 170170TF00 temper; 3000 kg
Tensile Strength, Ultimate 455 MPa66000 psiM01 temper
 545 MPa79000 psiTF00 temper
Tensile Strength, Yield  235 MPa
@Strain 0.5 %
34100 psi
@Strain 0.5 %
M01 temper
 370 MPa
@Strain 0.5 %
53700 psi
@Strain 0.5 %
TF00 temper
Elongation at Break 25 %25 %in 50 mm, M01 temper
Modulus of Elasticity 133 GPa19300 ksi
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Shear Strength 330 MPa47900 psiM01 temper
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000103 ohm-cm
@Temperature 20.0 °C
0.0000103 ohm-cm
@Temperature 68.0 °F
TF00 temper
 
Thermal PropertiesMetricEnglishComments
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 315 °C599 °FStress-Relieving Temperature; 1 h for each 25 mm of section thickness
Solution Temperature 885 °C1630 °F1 h for each 25 mm of section thickness
Aging Temperature 480 °C896 °F1 hour
Precipitation Temperature 482 °C
@Time 3600 sec
900 °F
@Time 1.00 hour
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.50 - 2.0 %0.50 - 2.0 %
Copper, Cu 90.4 %90.4 %
Iron, Fe 1.0 - 3.0 %1.0 - 3.0 %
Lead, Pb <= 0.25 %<= 0.25 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni 1.0 - 3.5 %1.0 - 3.5 %
Silicon, Si 0.50 - 2.0 %0.50 - 2.0 %
Zinc, Zn 0.50 - 5.0 %0.50 - 5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NDZ-S, UNS C99500, Copper Casting Alloy
Aluminum Bronze, UNS C95300, Casting Alloy, As Cast
Aluminum Bronze, UNS C95300 Casting Alloy, TQ50 Temper
UNS C99300, Copper Casting Alloy
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast

MC99400b1 / 11984

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.