MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Bronze, UNS C95300 Casting Alloy, TQ50 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Heat treatable. Except where noted, all property values listed below are for sand casting.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Electrical applications, pickling baskets, nuts, gears, steel mill slippers, marine equipment, welding jaws, non-sparking hardware.

Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9B

Tempering: Solution treated at 855°C (1575°F), quenched, tempered 2 hours at 620°C (1150°F).

Key Words: Aluminum bronze, ASTM B148, ASTM B148-9B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1741743000 kg
Hardness, Rockwell B 8181
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 275 MPa39900 psi
Elongation at Break 12 %12 %in 50 mm
Reduction of Area 14 %14 %
Modulus of Elasticity 110 GPa16000 ksi
Compressive Strength 825 MPa120000 psi
Poissons Ratio 0.3140.314
Machinability 55 %55 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.0 GPa6090 ksi
Charpy Impact 37.0 J
@Temperature -20.0 - 100 °C
27.3 ft-lb
@Temperature -4.00 - 212 °F
Keyhole
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000133 ohm-cm
@Temperature 20.0 °C
0.0000133 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.071.078 kA/m field strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 63.0 W/m-K
@Temperature 20.0 °C
437 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 595 - 650 °C1100 - 1200 °F
Solution Temperature 855 °C1570 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 9.0 - 11 %9.0 - 11 %
Copper, Cu >= 86 %>= 86 %
Iron, Fe 0.80 - 1.5 %0.80 - 1.5 %
Other, total <= 1.0 %<= 1.0 %
 
Descriptive Properties
Elastic Limit125 MPaas cast
 205 MPaTQ50 temper

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95300, Casting Alloy, As Cast
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
AISI 4142 Steel, Annealed and Cold Drawn
Beryllium Copper, UNS C17200, TD04 Temper rod, bar, plate, tubing, 9.5-25 mm
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper

MC95300b2 / 193497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.