MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Springflex Spring Wire
Categories: Metal; Ferrous Metal; Austenitic; Ferritic; Stainless Steel

Material Notes: Sandvik Springflex is a duplex (austenitic-ferritic) stainless steel characterized by:
  • Very good fatigue resistance
  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • High resistance to stress corrosion cracking (SCC) in environments containing hydrogen sulphide
  • High resistance to general corrosion, pitting, and crevice corrosion
  • High resistance to erosion corrosion and corrosion fatigue
  • Physical properties that offer design advantages
Service temperature: -100 to 300°C (-150 to 570°F)

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 700 - 900 MPaAnnealed wire
 900 - 1800 MPaFlat wire
 1350 - 1550 MPa
@Diameter 5.00 - 8.00 mm
 1450 - 1650 MPa
@Diameter 3.50 - 5.00 mm
 1550 - 1750 MPa
@Diameter 2.00 - 3.50 mm
 1700 - 1900 MPa
@Diameter 1.25 - 2.00 mm
 1800 - 2000 MPa
@Diameter 0.800 - 1.25 mm
 1900 - 2100 MPa
@Diameter 0.500 - 0.800 mm
 2000 - 2200 MPa
@Diameter 0.300 - 0.500 mm
 2100 - 2300 MPa
@Diameter 0.200 - 0.300 mm
 2150 - 2350 MPa
@Diameter 0.150 - 0.200 mm
Tensile Strength, Yield 350 - 550 MPa
@Strain 0.2 %
Annealed wire
 765 - 1530 MPa
@Strain 0.2 %
Flat wire
 1135 - 1335 MPa
@Diameter 5.00 - 8.00 mm,
Strain 0.2 %
 1220 - 1420 MPa
@Diameter 3.50 - 5.00 mm,
Strain 0.2 %
 1305 - 1505 MPa
@Diameter 2.00 - 3.50 mm,
Strain 0.2 %
 1430 - 1630 MPa
@Diameter 1.25 - 2.00 mm,
Strain 0.2 %
 1515 - 1715 MPa
@Diameter 0.800 - 1.25 mm,
Strain 0.2 %
 1600 - 1800 MPa
@Diameter 0.500 - 0.800 mm,
Strain 0.2 %
 1685 - 1885 MPa
@Diameter 0.300 - 0.500 mm,
Strain 0.2 %
 1770 - 1970 MPa
@Diameter 0.200 - 0.300 mm,
Strain 0.2 %
 1815 - 2015 MPa
@Diameter 0.150 - 0.200 mm,
Strain 0.2 %
Modulus of Elasticity 200 GPaas delivered
 205 GPatempered
Poissons Ratio 0.30as delivered; Calculated
 0.30Tempered; Calculated
Shear Modulus 77.0 GPaas delivered
 79.0 GPatempered
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000840 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 30.0 - 200 °C
Cold worked
 11.5 µm/m-°C
@Temperature 30.0 - 300 °C
Cold worked
 12.0 µm/m-°C
@Temperature 30.0 - 400 °C
Cold worked
 12.5 µm/m-°C
@Temperature 30.0 - 100 °C
Cold worked
 13.0 µm/m-°C
@Temperature 30.0 - 100 °C
Aged
 13.5 µm/m-°C
@Temperature 30.0 - 200 °C
Aged
 13.5 µm/m-°C
@Temperature 30.0 - 300 °C
Aged
 14.0 µm/m-°C
@Temperature 30.0 - 400 °C
Aged
Specific Heat Capacity 0.500 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 16.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 200 °C
 19.0 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air -100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 22 %
Manganese, Mn 0.90 %
Molybdenum, Mo 3.2 %
Nickel, Ni 5.0 %
Nitrogen, N 0.18 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.50 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik 11R51 Spring Wire
316 Stainless Steel, spring tempered wire, 13 mm diam.
Sandvik 12R10L Spring wire
Sandvik Sanicro 75X Spring Wire
Sandvik Springflex SF Spring Wire

NSANDV5232 / 199796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.