MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 12R10L Spring wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik 12R10L is an austenitic stainless steel with a very low cobalt content, especially suitable for nuclear applications. The grade is characterized by moderate tensile strength, high corrosion resistance and moderate fatigue and relaxation resistance. It has very good ductility and a clean structure with low nonmetallic inclusions. Service temperature: -200 to 250°C (330 to 480°F)

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  750 MPa
@Diameter 0.200 - 0.300 mm
109000 psi
@Diameter 0.00787 - 0.0118 in
 1075 MPa
@Diameter 8.50 - 10.0 mm
155900 psi
@Diameter 0.335 - 0.394 in
 1120 MPa
@Diameter 7.00 - 8.50 mm
162000 psi
@Diameter 0.276 - 0.335 in
 1160 MPa
@Diameter 6.00 - 7.00 mm
168000 psi
@Diameter 0.236 - 0.276 in
 1205 MPa
@Diameter 5.00 - 6.00 mm
174800 psi
@Diameter 0.197 - 0.236 in
 1250 MPa
@Diameter 4.25 - 5.00 mm
181000 psi
@Diameter 0.167 - 0.197 in
 1290 MPa
@Diameter 3.50 - 4.25 mm
187000 psi
@Diameter 0.138 - 0.167 in
 1330 MPa
@Diameter 3.00 - 3.50 mm
193000 psi
@Diameter 0.118 - 0.138 in
 1375 MPa
@Diameter 2.50 - 3.00 mm
199400 psi
@Diameter 0.0984 - 0.118 in
 1420 MPa
@Diameter 2.00 - 2.50 mm
206000 psi
@Diameter 0.0787 - 0.0984 in
 1465 MPa
@Diameter 1.75 - 2.00 mm
212500 psi
@Diameter 0.0689 - 0.0787 in
 1505 MPa
@Diameter 1.50 - 1.75 mm
218300 psi
@Diameter 0.0591 - 0.0689 in
 1550 MPa
@Diameter 1.25 - 1.50 mm
225000 psi
@Diameter 0.0492 - 0.0591 in
 1590 MPa
@Diameter 1.00 - 1.25 mm
231000 psi
@Diameter 0.0394 - 0.0492 in
 1635 MPa
@Diameter 0.800 - 1.00 mm
237100 psi
@Diameter 0.0315 - 0.0394 in
 1680 MPa
@Diameter 0.650 - 0.800 mm
244000 psi
@Diameter 0.0256 - 0.0315 in
 1720 MPa
@Diameter 0.500 - 0.650 mm
249000 psi
@Diameter 0.0197 - 0.0256 in
 1760 MPa
@Diameter 0.400 - 0.500 mm
255000 psi
@Diameter 0.0157 - 0.0197 in
 1810 MPa
@Diameter 0.300 - 0.400 mm
263000 psi
@Diameter 0.0118 - 0.0157 in
 1890 MPa
@Diameter 0.150 - 0.200 mm
274000 psi
@Diameter 0.00591 - 0.00787 in
Tensile Strength, Yield 800 - 2200 MPa116000 - 319000 psiFlat wire
 1345 MPa
@Diameter 8.50 - 10.0 mm
195100 psi
@Diameter 0.335 - 0.394 in
 1400 MPa
@Diameter 7.00 - 8.50 mm
203000 psi
@Diameter 0.276 - 0.335 in
 1450 MPa
@Diameter 6.00 - 7.00 mm
210000 psi
@Diameter 0.236 - 0.276 in
 1505 MPa
@Diameter 5.00 - 6.00 mm
218300 psi
@Diameter 0.197 - 0.236 in
 1560 MPa
@Diameter 4.25 - 5.00 mm
226000 psi
@Diameter 0.167 - 0.197 in
 1615 MPa
@Diameter 3.50 - 4.25 mm
234200 psi
@Diameter 0.138 - 0.167 in
 1665 MPa
@Diameter 3.00 - 3.50 mm
241500 psi
@Diameter 0.118 - 0.138 in
 1720 MPa
@Diameter 2.50 - 3.00 mm
249000 psi
@Diameter 0.0984 - 0.118 in
 1775 MPa
@Diameter 2.00 - 2.50 mm
257400 psi
@Diameter 0.0787 - 0.0984 in
 1830 MPa
@Diameter 1.75 - 2.00 mm
265000 psi
@Diameter 0.0689 - 0.0787 in
 1880 MPa
@Diameter 1.50 - 1.75 mm
273000 psi
@Diameter 0.0591 - 0.0689 in
 1935 MPa
@Diameter 1.25 - 1.50 mm
280600 psi
@Diameter 0.0492 - 0.0591 in
 1990 MPa
@Diameter 1.00 - 1.25 mm
289000 psi
@Diameter 0.0394 - 0.0492 in
 2045 MPa
@Diameter 0.800 - 1.00 mm
296600 psi
@Diameter 0.0315 - 0.0394 in
 2095 MPa
@Diameter 0.650 - 0.800 mm
303900 psi
@Diameter 0.0256 - 0.0315 in
 2150 MPa
@Diameter 0.500 - 0.650 mm
312000 psi
@Diameter 0.0197 - 0.0256 in
 2200 MPa
@Diameter 0.400 - 0.500 mm
319000 psi
@Diameter 0.0157 - 0.0197 in
 2260 MPa
@Diameter 0.300 - 0.400 mm
328000 psi
@Diameter 0.0118 - 0.0157 in
 2310 MPa
@Diameter 0.200 - 0.300 mm
335000 psi
@Diameter 0.00787 - 0.0118 in
 2365 MPa
@Diameter 0.150 - 0.200 mm
343000 psi
@Diameter 0.00591 - 0.00787 in
Modulus of Elasticity 185 GPa26800 ksidelivered
 190 GPa27600 ksitempered
Poissons Ratio 0.300.30delivered; Calculated
 0.300.30Tempered; Calculated
Shear Modulus 71.0 GPa10300 ksidelivered
 73.0 GPa10600 ksitempered
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000800 ohm-cm
@Temperature 20.0 °C
0.00000800 ohm-cm
@Temperature 68.0 °F
 0.00000850 ohm-cm
@Temperature 100 °C
0.00000850 ohm-cm
@Temperature 212 °F
 0.00000900 ohm-cm
@Temperature 200 °C
0.00000900 ohm-cm
@Temperature 392 °F
 0.00000950 ohm-cm
@Temperature 300 °C
0.00000950 ohm-cm
@Temperature 572 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.5 µm/m-°C
@Temperature 20.0 - 200 °C
9.72 µin/in-°F
@Temperature 68.0 - 392 °F
 18.5 µm/m-°C
@Temperature 20.0 - 300 °C
10.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 50.0 - 100 °C
0.120 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity  15.0 W/m-K
@Temperature <=20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature <=68.0 °F
 16.0 W/m-K
@Temperature <=100 °C
111 BTU-in/hr-ft²-°F
@Temperature <=212 °F
 18.0 W/m-K
@Temperature <=200 °C
125 BTU-in/hr-ft²-°F
@Temperature <=392 °F
 19.0 W/m-K
@Temperature <=300 °C
132 BTU-in/hr-ft²-°F
@Temperature <=572 °F
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -200 °C-328 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.080 %0.080 %
Chromium, Cr 18 %18 %
Cobalt, Co <= 0.050 %<= 0.050 %
Manganese, Mn 1.2 %1.2 %
Nickel, Ni 9.0 %9.0 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.60 %0.60 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik 5R10 Spring wire
Sandvik 9RU10 Spring Wire
316 Stainless Steel, spring tempered wire, 13 mm diam.
316 Stainless Steel, spring tempered wire, 1.6 mm diam.
Overview of materials for Cobalt Alloy

NSANDV5065 / 199629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.