Scotchkote Epoxy Coating 175SR has been specifically developed as at 100% solids lining for the internals of tanks, vessels and other equipment in contact with aromatic hydrocarbon solvents, ethanol and some chlorinated solvents. Product Features: - Is designed for application in a single coat by plural feed hot spray. The product can also be applied by brush or squeegee.
- Is primarily intended for use on steel but can also be used on concrete surfaces with the appropriate primer.
- Suitable for continuous immersion in aromatic hydrocarbon solvents, ethanol and some chlorinated solvents.
- Excellent adhesion and abrasion resistance.Information provided by 3M
|