MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear® DEXRON® III & MERCON® Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear DEXRON® III & MERCON® Automatic Transmission Fluid is a multipurpose fluid for the electronically controlled transmissions of most domestic and imported automobiles, trucks and buses built after 1989. It is approved by GM as a DEXRON III fluid and by Ford as a MERCON fluid. It is recommended for Ford transmissions requiring Type CJ and Type H fluids. It is approved by Allison as a C-4 fluid and also can be used in off-highway transmissions, power steering systems and other hydraulic systems. Hydroclear DEXRON III & MERCON Automatic Transmission Fluid is suited for a wide variety of industrial applications that call for an ISO 46 or SAE 20W hydraulic fluid. It qualifies as a Denison HF-O hydraulic fluid and has performed well in both Sunstrand and Vickers hydraulic pumps. Hydroclear DEXRON III & MERCON Automatic Transmission Fluid improves shifting characteristics at both high- and low-ambient temperatures. It resists thermal and oxidative degradation and offers outstanding low-temperature fluidity. It inhibits the formation of gum, sludge, lacquer and foam, protecting transmission from rust, corrosion and wear. It is dyed red for easy identification.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 33.3 °
Viscosity 14900 cP
@Temperature -40.0 °C
Viscosity Measurement 197Viscosity Index
Kinematic Viscosity at 40°C (104°F) 33 cSt
Kinematic Viscosity at 100°C (212°F) 7.7 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °F
Flash Point 374 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Moly Poly Grease NLGI No. 2
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid

WCON028 / 75065

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.