MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 Moly Poly Grease NLGI No. 2
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Moly Poly Grease is a long-life, lithium 12-hydroxy grease for chassis, wheel bearings, ball joints, U-joints, tie-rod ends, steering knuckles and brake self-adjusting screws found in automobiles, trucks and farm and off-road equipment. Its polyethylene and molybdenum content reduces wear and noise. The combination of solid lubricants (moly and poly) with light viscosity base oil make this grease an excellent choice for high-speed antifriction bearings subject to shock loading and for use year round in most climates. Specifically designed as an excellent chassis grease for the transportation industry, Moly Poly Grease meets Ford ESA-MIC75-B and Mack MG-C specifications.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9393Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 533 SUS533 SUSBase Oil Property
Saybolt Viscosity at 210°F 76 SUS76 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 151 cSt151 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 14.4 cSt14.4 cStBase Oil
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 4444
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)
Four Ball Wear 0.400 mm0.0157 inEP
Penetration <= 330<= 330Worked 1,000,000 strokes
Penetration P(60), 1/10 mm 280280
Timken Test 27200 g60.0 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 138 °C280 °F
Minimum Service Temperature, Air -20.6 °C-5.00 °F
Pour Point -15.0 °C5.00 °F(Base Oil Property)
Dropping Point 193 °C380 °F
 
Descriptive Properties
ASTM Rust A&BPass
ColorGray-Black
Film Strength DurabilityPass8 hrs. at 10 lb. Load
 Pass
Film Strength Durability Scar Width0.9 mm
Molybdenum Disulfide1 wt.%
Oil SeparationMax 12 mlat 96 hrs.
Oxidation Stability19.6 psi drop after 1000 hrs
Penetration After Oxidation+20
Polyethylene5 wt.%
Soap Type (Thickener)Lithium
Stringiness TestMax 25 mm
Timken Cup Corrosion TestNo Rust300 hours at 77°F
Water Washout10 wt.%at 176°F
Wheel Bearing Leakage1.9 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ConocoPhillips Hydroclear® DEXRON® III & MERCON® Automatic Transmission Fluid
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid

WCON213 / 75250

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.