MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Crastin® ST830FRUV NC010 PBT-HIFR(17)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Unreinforced, Flame Retardant, UV Stabilized, Polybutylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183
Melt Density 1.17 g/cc
@Temperature 250 °C
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4, 2577
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 41.0 MPaISO 527-1/-2
Elongation at Break 45 %Nominal; ISO 527-1/-2
Elongation at Yield 9.0 %ISO 527-1/-2
Tensile Modulus 2200 MPaISO 527-1/-2
Flexural Modulus 2100 MPaISO 178
Poissons Ratio 0.39
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 220 kJ/m²
@Temperature -40.0 °C
ISO 180/1U
 220 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
 NB
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 350 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 350 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 36.0 kV/mmIEC 60243-1
Dissipation Factor 0.00109
@Frequency 100 Hz
IEC 62631-2-1
 0.024
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 190 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 190 µm/m-°CISO 11359-1/-2
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.850 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
Oxygen Index 27 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °COptimum, Injection
 240 - 260 °CRange, Injection
Mold Temperature 80.0 °COptimum, Injection
 30.0 - 130 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %Injection
Hold Pressure >= 60.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassDNIISO 3795 (FMVSS 302)
Part Marking Code>PBT-HIFR(17)<ISO 11469
PolymerPBT-I FR(17)
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPBT-HIFR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® T835FRUV NC010 PBT
Celanese Hytrel® DYM250S BK472 TPC-ET+PBT
Celanese Crastin® S650FR NC010 PBT-FR(17)
Celanese Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
Celanese Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)

PDSX5076 / 197716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.